Kaʻina Hana Pepa PET
Mea maka o ka pepa PET #pet sheet extrusion
ʻO ka pepa PET, e like me nā plastics ʻē aʻe, pili pili ka hana i ke kaumaha molekala, a ʻo ka viscosity hiʻohiʻona e hoʻoholo ai i ke kaumaha mole. ʻOi aku ka maikaʻi o ka viscosity intrinsic, ʻoi aku ka maikaʻi o ke kino a me nā waiwai kemika. akā, ʻo ka maikaʻi ʻole o ka wai, ka hopena i ka paʻakikī. ʻO ka haʻahaʻa o ka viscosity intrinsic, ʻoi aku ka maikaʻi o nā waiwai physicochemical a me ka ikaika hopena. No laila, pono e koho ʻia ʻo 0.8dl/G-0.9dL /g no ke ʻano viscosity o ke kiʻi ʻoniʻoni ʻo PET.

Kaʻina hana PET #extrusora de garrafa pet
ʻO nā mea hana nui o ka PET transparent sheet: crystallization tower, drying tower, extruder, poʻo mold, ʻekolu-roll calender a me ka coiler.
Penei ke kaʻina hana: crystallization maka → maloʻo → extrusion plasticizing → extrusion molding → calendering molding → winding products.
ʻO ka hana mua ka crystallization. Hoʻomaʻamaʻa ʻia nā ʻāpana PET i loko o ka hale kiaʻi crystallization, no laila ua hoʻonohonoho pono ʻia nā molekala, a laila hoʻokiʻekiʻe ʻia ka mahana hoʻololi aniani o nā ʻāpana, i manaʻo ʻia e pale i ka adhesion i ka wā o ka hoʻomaloʻo ʻana a me ka pale ʻana i ka hopper. He hana koʻikoʻi ka crystallization, e lawe ana i 30 mau minuke a i 90 mau minuke, a ʻoi aku ka mahana ma lalo o 149 ° C.
Kaʻanuʻuʻelua, maloʻo. Ma muli o ka hydrolytic degradation o PET i hoʻokumu ʻia e ka wai ma lalo o nā kūlana wela kiʻekiʻe, ua hoʻemi ʻia kona ʻano adhesion, a ʻo kona mau kino kino, ʻoi aku ka ikaika o ka hopena, e hoʻemi ʻia me ka hōʻemi ʻana o ke kaumaha mole. No laila, pono e hoʻomaloʻo ʻia ka PET ma mua o ka hoʻoheheʻe ʻana a me ka extrusion e hōʻemi i ka ʻike o ka wai, a ʻoi aku ka liʻiliʻi ma mua o 0.005%. Ma muli o ka waiwai hygroscopic o ka mea PET, ʻo ka wai i loko o ka ʻili o ka ʻāpana e hana i nā paʻa molekala, a e noho kekahi wai i loko o ka ʻāpana, e hopena i nā pilikia maloʻo, no laila ʻaʻole hiki ke hoʻohana ʻia ka ea wela. Pono ka hau o ka ea wela ma lalo o -40 ° C, a hele ka ea wela ma ke kaapuni paʻa i ka hopper maloʻo no ka maloʻo mau. #pe mīkini extruder.


ʻO nā kiʻi i hōʻike ʻia mai ka hale kūʻai o JWELL Turkey i Kepakemapa. Ma hope o ka hoʻouna ʻana mai ka hale hana ʻo Jwell i ka hale kūʻai o ka mea kūʻai aku ʻo Turkey, ua hele ʻo Jwell engineer i ka hale hana e hoʻokomo i ka mīkini PET sheet extrusion no ka thermoforming packaging. #rpet hana ʻana i ka plastic

ʻO ke kolu o ka ʻanuʻu he extrusion molding. Hoʻololi ʻia ʻo PET i polymer me ka helu heheʻe ma hope o ka crystallization a me ka maloʻo ʻana, a ʻoi aku ka kiʻekiʻe o ka mahana o ka polymer a he haiki ka pae hoʻomalu wela. Hoʻokaʻawale ʻia nā ʻāpana i hoʻoheheʻe ʻole ʻia mai ka hoʻoheheʻe ʻana me ka hoʻohana ʻana i ka pale pale i hoʻolālā kūikawā ʻia no ka polyester, e kōkua ana i ka mālama ʻana i kahi kaʻina ʻāhi lōʻihi a hoʻonui i ka puka o ka extruder. Hoʻohana ʻia ke poʻo lehelehe maʻalahi me ke koʻokoʻo hoʻopaʻa laina kahe, he conical ke poʻo, ʻo ke kahawai kahe streamlined a me ka lehelehe make ʻole e hōʻike i ka maikaʻi o ka lau, ʻo ka mea wela o ke poʻo ka hana o ka hoʻokahe a me ka hoʻomaʻemaʻe, ka poʻo make lehelehe lehelehe pono e hōʻoia maikaʻi like like, ke poʻo make lehelehe like ole pili pono i ka transverse mānoanoa deviation o ka pepa a me ka palahalaha o ka calendering. ʻO ka mahana e pili ana i ka mua, ka waena waena o ka fuselage, ka hope o ka fuselage, ka mea hoʻololi upena a me ke poʻo i kēlā me kēia 240 ° C-260 ° C, 265 ° C-275 ° C, 260 ° C- 265°C, 260°C-265°C, 255°C-265°C. #mekini pepa pipi

KaʻAnuʻu ʻehā: Hoʻoluʻu a hoʻonohonoho. Ma hope o ka puka ʻana o ka heheʻe mai ke poʻo pololei i loko o ka kalena ʻekolu ʻōwili no ka kalena a me ka hoʻomaha ʻana, mālama ʻia ka mamao ma waena o ka kalena ʻekolu ʻōwili a me ke poʻo ma kahi o 8cm, no ka mea inā nui ka mamao, maʻalahi ka pepa. e hāʻule a me nā wrinkles, e hopena i ka pau ʻole o ka pepa. Eia kekahi, ma muli o ka mamao loa, ua lohi loa ka hoʻoheheʻe ʻana o ka wela a keʻokeʻo ka crystallization, ʻaʻole kūpono i ka calendering. ʻO ka ʻāpana kalena ʻekolu ʻekolu o luna, waena a me lalo ʻekolu mau wili, ua paʻa ka laina waena, a hiki ke hoʻoneʻe ʻia ke axis o nā wili ʻelua i luna a i lalo i ka wā i 40 ° C ka mahana o ka ʻōwili. -50°C i ka manawa hooluolu. Ma ka neʻe ʻana i luna a i lalo i ke koʻi e hoʻoponopono i ka ʻāpana ʻōwili, ʻo ka mahana o nā ʻōwili ʻelua o luna a me lalo he 30 ° C-60 ° C, 52 ° C-68 ° C, ʻo ia hoʻi, pono e hōʻoia nā wili ʻekolu i ka wikiwiki. synchronized, ʻoi aku ka wikiwiki ma luna o ka wikiwiki extrusion, ʻo ke kumu e hoʻopau i ka hoʻonui ʻana o ka mea e waiho ana i ka make a hoʻonāwaliwali i ke koʻikoʻi o loko o ka pepa, i nalowale nā wrinkles. E hoʻopuka ʻo PET i ka crystallization ma waena o 100 ° C a 250 ° C, a ʻo ka helu crystallization ʻo 140 ° C a 180 ° C ke wikiwiki, no laila hiki ke hoʻopau ʻia ka crystallization i loko o kekahi mau kekona. Pono ʻo PET e hele wikiwiki i kēia wahi wela crystallization a hoʻopaʻa paʻa i ka wela ʻekolu-roll.
KaʻAnuʻu ʻelima: Huki a kaʻa. Puka mai ka pepa ma o ka wili calender a komo i ka mea traction ma o ka roller guide. Hoʻokumu ʻia ka mea hoʻoheheʻe me ka ʻōwili pahu hana a me ka roller passive, a ʻo ke kaomi ʻana o nā wili ʻelua ka mea nui e pale ai i ka palahalaha i ka wā e huki ʻia ai ka lau e nā ʻōwili ʻelua i ka mea wili.